机械性能 |
硬度计硬度 |
|
ASTM D-2240 |
72 |
|
断裂伸长 |
|
ASTM D-638 |
360 |
% |
|
拉伸力 |
5%伸长 |
|
ASTM D-638 |
14 |
MPa |
10%伸长 |
|
ASTM D-638 |
20 |
MPa |
|
断裂拉伸力 |
|
ASTM D-638 |
45.8 |
MPa |
|
埃佐冲击强度 |
23℃ |
ASTM D-256 |
210 |
J/m |
|
揉曲模量 |
23℃ |
ASTM D-790 |
570 |
MPa |
|
初耐撕裂性能 |
|
ASTM D-1004 |
200 |
kn/m |
|
热性能 |
热畸变温度 |
@0.5MPa |
ASTM D-648 |
130 |
℃ |
维卡软化点 |
|
ASTM D-1525 |
207 |
℃ |
|
熔点 |
|
ASTM D-3418 |
218 |
℃ |
|
热畸变温度 |
@0.18MPa |
ASTM D-648 |
52 |
℃ |
|
其它性能 |
耐揉曲切口增长性能 |
|
ASTM D-1052 |
>3×104 |
|